Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Chlorobutyl 1066 Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Exxon Chemical
Trade Name Chlorobutyl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Chlorobutyl 1066 Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exxon™ Chlorobutyl rubber is a copolymer of isobutylene and isoprene. The product has characteristic specific gravity of 0.93. The product form is white to light amber bales.Information provided by ExxonMobil
Physical Properties Metric English Comments
Mooney Viscosity 38

@Temperature 125 °C
38

@Temperature 257 °F
ML 1+8, Target; ASTM D1646
33 - 43

@Temperature 125 °C
33 - 43

@Temperature 257 °F
ML 1+8; ASTM D1646
Maximum Moisture Content 0.30
0.30
ExxonMobil Method
Component Elements Properties Metric English Comments
Calcium, Ca 0.080 %
0.080 %
Target; ExxonMobil Method
0.050 - 0.11 %
0.050 - 0.11 %
ExxonMobil Method
Chlorine, Cl 1.26 %
1.26 %
Target; ExxonMobil Method
1.18 - 1.34 %
1.18 - 1.34 %
ExxonMobil Method
Processing Properties Metric English Comments
Cure Time 2.00 min
0.0333 hour
ts2, Target; ASTM D2084 (mod)
0.500 - 3.50 min
0.00833 - 0.0583 hour
ts2; ASTM D2084 (mod)
5.00 min
0.0833 hour
t'50, Target; ASTM D2084 (mod)
2.00 - 8.00 min
0.0333 - 0.133 hour
t'50; ASTM D2084 (mod)
12.0 min
0.200 hour
t'90, Target; ASTM D2084 (mod)
8.00 - 16.0 min
0.133 - 0.267 hour
t'90; ASTM D2084 (mod)
Descriptive Properties Value Comments
Antioxidant (non-staining) 0.02-0.12%
ExxonMobil Method
Rheometer 37-51 dN-m
ML, ASTM D2084 (mod)
44 dN-m
MH, Target, ASTM D2084 (mod)
Users viewing this material also viewed the following: