Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil EXXELOR™ PO 1020 Maleic anhydride functionalized polypropylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Elastomer, TPE , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name EXXELOR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil EXXELOR™ PO 1020 Maleic anhydride functionalized polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exxelor PO 1020 polymer resin is a high performance maleic anhydride fuctionalized homopolypropylene produced by reactive extrusion. It has been primarily designed to add polarity to polypropylene matrices and in particular improved polypropylene reactivity and amio-silane treated glass reinforcements. Its high content of maleic anhydride allows its use at low treat levels while maintaining optimum application properties.This grade is designed to:Function as a coupling agent between reinforcing materials, such as glass fibers and inorganic fillers, and polypropylene.Achieve compatibility in polypropylene/polyamide alloys.Achieve compatibility between polyolefins and more polar polymers that are capable of interaction with maleic anhydride for alloying recycling or co-extrusion purpose.Improve polypropylene-to-metal adhesion properties.Key Features: Performance enhancements in glass-filled polypropylene:Improved cost/performance balance compared to earlier generation modifiersEasy molding of highly glass-filled compounds and/or comples and thin parts due to its high flow peroperties. Outstandign unnotched Izod and Charpy performanceExcellent notched Izod and Charpy impact resistanceImproved tensile and flexural strengthAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 110 g/10 min

@Load 1.20 kg,
Temperature 190 °C
110 g/10 min

@Load 2.65 lb,
Temperature 374 °F
ASTM D1238
430 g/10 min

@Load 2.16 kg,
Temperature 190 °C
430 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Collected Volatile Condensable Material <= 0.30 %
<= 0.30 %
AM-S 350.03
Thermal Properties Metric English Comments
Melting Point 162 °C
324 °F
Peak; ExxonMobil Method
Optical Properties Metric English Comments
Yellow Index <= 30 %
<= 30 %
ASTM E313-96
Descriptive Properties Value Comments
Maleic anhydride graft level high
FTIR EPK-04 QT-02