Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LD-761 High EVA Compounding Resin  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-761 High EVA Compounding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer designed for high filler acceptance. Compounds produced from this resin have excellent flexibility and toughness.Applications: Specialty electrical compounds; Concentrates.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A; ASTM D1693
Melt Flow 5.7 g/10 min
5.7 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Hardness, Shore D 25
25
ASTM D2240
Tensile Strength, Ultimate 12.0 MPa
1740 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0210 GPa
3.05 ksi
1% Secant, ASTM D790
Tensile Impact Strength 742 kJ/m²
353 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 72.0 °C
162 °F
Exxon Method
Vicat Softening Point 48.0 °C
118 °F
1000g; ASTM D-1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved