ExxonMobil Escorene™ UL 12530CC Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 12530CC Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 12530CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot Melt Adhesives Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ExxonMobil method
Vinyl Acetate Content 30 %
30 %
ExxonMobil method
Melt Flow 130 g/10 min
130 g/10 min
ASTM D1238
Thermal Properties Metric English Comments
Melting Point <= 144 °C
<= 291 °F
Peak Melting Point; ExxonMobil method