ExxonMobil IPA Isopropyl Alcohol

Category Fluid
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil IPA Isopropyl Alcohol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.786 g/cc

@Temperature 20.0 °C
0.0284 lb/in³

@Temperature 68.0 °F
ASTM D4052
Kinematic Viscosity 2.61 cSt
2.61 cSt
ASTM D445
Vapor Pressure 0.0400 bar

@Temperature 20.0 °C
30.0 torr

@Temperature 68.0 °F
ExxonMobil Method
Thermal Properties Metric English Comments
Boiling Point 82.2 °C
180 °F
Initial; ASTM D1078
Flash Point 12.2 °C
54.0 °F
ASTM D56
Descriptive Properties Value Comments
Acidity 1E-05
as Acetic Acid, ExxonMobil Method
Dry Point 180°F
ASTM D86
Purity 1
ExxonMobil Method