ExxonMobil Jayflex™ DINP Plasticizer

Category Fluid
Manufacturer Exxon Chemical
Trade Name Jayflex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Jayflex™ DINP Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appearance: Clear and FreeAvailability: AmericasCAS Number: 33703-08-01Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.971 - 0.975 g/cc
0.0351 - 0.0352 lb/in³
BRCP 4843
Maximum Moisture Content 0.10
0.10
BRCP 5053
Descriptive Properties Value Comments
Acidity <0.01%
as phthalic acid, BRCCP 4625
Color <25
Platinum Cobalt, BRCP 4273
Ester Content >99.6%
BRCP 4360