ExxonMobil Label-Lyte™ 18LL-101 OPP Film

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte™ 18LL-101 OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling applications. This film is formulated with a proprietary non-migratory slip system. The treated clear layer provides excellent anchorage to most adhesives and is the intended print and laminating surfaces.Availability: Latin America, North America and South AmericaKey Features: Outstanding clarity and glossExcellent ink adhesion with most solvent-based and water-water-based ink systemsExcellent bond strength with most laminating adhesivesApplications:Beverage, CarbonatedBeverage, Mineral WatersDairy ProductsDry Foods and Beverage Powders Uses: Pressure Sensitive Labels Processing Method: Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Thickness 17.8 microns
0.700 mil
ExxonMobil Method
Coating Weight 15.7 g/m²
9.80 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 162 %
162 %
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 47 %
47 %
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Coefficient of Friction 0.20
0.20
Machinable; ExxonMobil Method
Film Tensile Strength at Break, MD 138 MPa
20000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 296 MPa
42900 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 5.5 %

@Temperature 135 °C
5.5 %

@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 6.0 %

@Temperature 135 °C
6.0 %

@Temperature 275 °F
ExxonMobil Method
Optical Properties Metric English Comments
Haze 1.8 %
1.8 %
ExxonMobil Method
Gloss 88 %
88 %
45°, Machinable Surface; ExxonMobil Method
Descriptive Properties Value Comments
Wetting Tension 0.85 receding cos theta
Print Surface
Yield 44000 in2/lb