Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte® 65 LIM-301 White Opaque OPP Film for Injection Mold Label Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
White, treated, polypropylene film designed for injection mold labeling. It provides the right combination of roughness, anti-static, printability, cutting, and stiffness properties for this demanding application. The treated print surface is designed for conventional and UV-cured offset lithography, solvent flexo, and gravure printing. This film has a smooth glossy appearance after molding, resulting in outstanding container graphics. Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Thickness 66.0 microns
2.60 mil
Coating Weight >= 46.1 g/m²
>= 28.8 lb/ream
520
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 180 %
180 %
510
Film Elongation at Break, TD 65 %
65 %
510
Coefficient of Friction 0.25
0.25
untreated side; 430
0.30
0.30
treated side; 430
Film Tensile Strength at Break, MD 100.77 MPa
14615 psi
510
Film Tensile Strength at Break, TD 151.15 MPa
21923 psi
510
Thermal Properties Metric English Comments
Shrinkage, MD 3.5 %
3.5 %
at 275°F; 438
Shrinkage, TD 1.3 %
1.3 %
at 275°F; 438
Optical Properties Metric English Comments
Gloss 10 %
10 %
untreated surface; 442
50 %
50 %
treated surface; 442
Transmission, Visible 15 %
15 %
417
Descriptive Properties Value Comments
Gurley Stiffness, MD, mgf 23
Gurley Stiffness, TD, mgf 39
Yield, in2/lb 15000