Material Notes:
Mobil Jet Oil 254 is a third-generation, extra high performance, synthetic aircraft-type gas turbine lubricant engineered to meet the performance requirements for gas turbine engines used in commercial and military aircraft.  This product is formulated from a specially prepared, hindered-ester base stock and fortified with a unique chemical additive package. The result is a product having superior thermal and oxidation stability that resists deterioration and deposit formation while maintaining the physical characteristics required by builder and military specifications.  The physical properties of Mobil Jet Oil 254 are similar to those currently available, earlier-generation gas turbine lubricants. The effective operating range of  the lubricant is between -40°C (-40 °F) and 232°C (450°F).Mobil Jet Oil 254 is recommended for aircraft gas turbine engines of the turbo-jet, turbo-fan, turbo-prop, and turbo-shaft (helicopter) types used in commercial and military service.  It is also suitable for aircraft-type gas turbine engines used in industrial or marine applications. Mobil Jet Oil 254 is approved against the High Thermal Stability (HTS) classification of U.S. Military Specification MIL-PRF-23699.  It is also compatible with other synthetic gas turbine lubricants meeting MIL-PRF-23699.  However, mixing with other products is not recommended because the blend would result in some loss of the superior performance characteristics of Mobil Jet Oil 254. Mobil Jet Oil 254 is completely compatible with all metals used in gas turbine construction, as well as with F Rubber (Viton A), H Rubber (Buna N), and other commonly used seal materials.
Physical Properties Metric English Comments
Specific Gravity 1.0044 g/cc
1.0044 g/cc
Viscosity Measure 11500 cSt

@Temperature -40.0 °C
11500 cSt

@Temperature -40.0 °F
Kinematic Viscosity; ASTM D445
Kinematic Viscosity at 40°C (104°F) 26.4 cSt
26.4 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 5.30 cSt
5.30 cSt
-2.2 change @ -40°C after 72 hours; ASTM D445
Evaporation Loss 2.1 %
2.1 %
6.5 hr @ 204 C, 29.5" Hg
7.4 %
7.4 %
6.5 hr @ 232 C, 19.5" Hg
25.2 %
25.2 %
6.5 hr @ 232 C, 5.5" Hg
Thermal Properties Metric English Comments
Pour Point -62.0 °C
-79.6 °F
ASTM D97
Flammability Test 288
288
Fire Point [°C]
399
399
Auto Ignition [°C]
Flash Point 254 °C
489 °F
ASTM D92
Chemical Properties Metric English Comments
Total Acid Number 0.080
0.080
mgKOH/g
Descriptive Properties Value Comments
Foam Sequence I, ASTM D1131 0/0
Foam Sequence II, ASTM D893 10/0
Foam Sequence III, ASTM D893 8/0
Foam Stability, after 1 min settling, mL 0
Rubber Swell, % 20
H Rubber, 72 hr @ 70°C
20.8
F Rubber, 72 hr @ 204°C
Ryder Gear, Ave, lb/in % Hercolube A 2715144
Sonic Shear Stability, KV change % 0.7
@ 40°C