ExxonMobil Mobilith AW Series 0

Category Fluid , Lubricant , Lithium Gellant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobilith AW Series 0.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and shock loading. Oxidation inhibitors enhance the ability of Mobilith AW Series greases to withstand operating temperatures up to 175º C with minimum breakdown or leakage. Rust inhibitors protect lubricated components from rust and corrosion. Mobilith AW Series greases are available in NLGI grades from 00 to 3 with base oil viscosity ISO VG 150, except for Mobilith AW 00 which is ISO VG 100. Mobilith AW Series greases have excellent handling and dispensing properties at temperatures down to -40º C, which means they are superior to most high-temperature greases that generally have poorer low-temperature consistency and pumpability. The Mobilith AW Series greases provide superior lubrication under thin film conditions, and resist displacement from highly loaded components encountered in industrial applications. Their excellent resistance to water and protection against rust make the greases well suited to applications requiring maximum protection over extended periods.Application Considerations: In order to maintain the performance characteristics of the Mobilith AW Series greases, completely clean or purge previously used greases from the system. Mobilith AW Series greases are heavy-duty products designed for multi-purpose industrial applications covering a wide range of operating conditions. Specific applications include: Mobilith AW 1, 2, and 3 greases are recommended for the lubrication of bearings operating with heavy or shock loads, and at temperatures up to 175º C. They are suitable for lubricating cams, ways, and other sliding elements. Other applications include vehicles and greased components in paper mills, where both water and high temperatures are encountered; Mobilith AW 0 and 00 are softer, high-temperature greases recommended for centralised grease application systems, gear lubrication, and where extreme-cold-temperature pumpability is important
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 150 cSt
150 cSt
ASTM D445
Oxidative Stability 100 hour
100 hour
Pressure Drop of 35 kPa; ASTM D942
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
Four Ball Wear 0.500 mm
0.0197 in
ASTM D2266
Penetration 370
370
Worked, 25°C; ASTM D217
Timken Test >= 18100 g
>= 40.0 lb
Descriptive Properties Value Comments
Color green
Copper Strip Corrosion, ASTM D4048 1A
Corrosion Prevention, ASTM D1743 pass
Emcor/SKF Water Wash Test, IP 220 0
Soap/Thickener Type lithium complex