Material Notes:
Product Description: A one-side sealable OPP film with a translucent white appearance. STW-RH is designed to run on multi-lane ice cream novelty equipment. This film exhibits excellent machining performance in elevated relative humidity dairy environments.Availability: Latin America, North America and South AmericaKey Features:Excellent stiffness Low seal initiationRobust machinability in humid environmentsOutstanding high gloss, translucent appearanceMinimal product movement during packagingFeatures:In Lamination Lap SealableApplications:Dairy ProductsIce Cream Uses:HFFS Flexible PackagingPre-made Bags – Flexible PackagingVFFS Flexible PackagingProcessing Method: Inner Web Adhesive LaminationInformation provided by ExxonMobil
Physical Properties Metric English Comments
Water Vapor Transmission 4.19 g/m²/day

@Temperature 38.0 °C
0.270 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
Thickness 35.6 microns
1.40 mil
ExxonMobil Method
Coating Weight 28.2 g/m²
17.6 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.39
0.39
Machinable; ExxonMobil Method
Film Tensile Strength at Break, MD 98.6 MPa
14300 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 231 MPa
33500 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 5.0 %

@Temperature 135 °C
5.0 %

@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 5.0 %

@Temperature 135 °C
5.0 %

@Temperature 275 °F
ExxonMobil Method
Optical Properties Metric English Comments
Gloss 65 %
65 %
45°, Machinable Surface; ExxonMobil Method
Transmission, Visible 50 %
50 %
ExxonMobil Method
Descriptive Properties Value Comments
Crimp Seal MST 205°F
Sealable
Crimp Seal Strength 500 g/in
Sealable, 260°F, 20 psi, 0.8 sec
Opacity 0.6
Yield 24500 in2/lb