ExxonMobil PP7654KNE2 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP7654KNE2 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded large consumer and industrial parts.Availability: North America Features: Good ColorabilityGood Dimensional StabilityGood Mold ReleaseGood Thermal StabilityMedium Impact ResistanceUses: Automotive Applications Consumer Applications Household Goods Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.2 MPa
3220 psi
2.0 in/min; ASTM D638
Elongation at Yield 4.6 %
4.6 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1230 MPa
179000 psi
0.05 in/min; ASTM D790A
1380 MPa
200000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched NB
NB
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C
206 °F
ASTM D648