Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 101-55W255 Thermoplastic Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 101-55W255 Thermoplastic Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for use in residential dishwasher applications and contains a stabilization system for protection against copper and other metal-catalyzed degradation. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Key Features:UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified for Canada - Component.EU and China RoHS compliant.Applications:Appliance-Dishwasher Seals and GasketsUses:Appliance ComponentsGasketsSealsProcessing Method: Coextrusion, Injection Molding, Profile Extrusion, Extrusion, Multi Injection Molding and Sheet ExtrusionAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 59

@Time 15.0 sec
59

@Time 0.00417 hour
2 mm; ISO 868
Tensile Strength at Break 4.70 MPa
682 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 1.80 MPa

@Strain 100 %
261 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 430 %
430 %
Across Flow; ASTM D412 and ISO 37
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
UL File Number - E80017
Users viewing this material also viewed the following: