Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 151-70W256 Thermoplastic Vulcanizate - Flame Retardant

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 151-70W256 Thermoplastic Vulcanizate - Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A soft, black, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has been designed to meet the Underwriter Laboratories (UL) Subjects 6703, UL 6703A and UL 1703 material requirements for both junction boxes and connectors (both enclosure and insulation) for use in photovoltaic systems. The flame retardants used are RoHS compliant and provide UL 94 flammability classifications of V-1 down to a thickness of 1.5 mm and 5VA down to a thickness of 1.8 mm. The material has an elevated Relative Thermal Index (RTI) of 90°C and meets the requirements for suitability for outdoor use with an (f1) rating. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.Key Features:Suitability for outdoor use.EU and China RoHS compliant.UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
2 mm; ISO 868
Tensile Strength at Break 4.80 MPa
696 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 2.30 MPa

@Strain 100 %
334 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 480 %
480 %
Across Flow; ASTM D412 and ISO 37
Thermal Properties Metric English Comments
UL RTI, Electrical 90.0 °C
194 °F
UL 746
UL RTI, Mechanical without Impact 90.0 °C
194 °F
UL 746
Flammability, UL94 V-1

@Thickness 1.50 - 3.00 mm
V-1

@Thickness 0.0591 - 0.118 in
UL File Number - E80017
5VA

@Thickness 1.80 mm
5VA

@Thickness 0.0709 in
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
Oxygen Index 24 %
24 %
ASTM D2863 and ISO 4589-2
Electrical Properties Metric English Comments
Dielectric Strength 28.3 kV/mm

@Thickness 2.03 mm
720 kV/in

@Thickness 0.0799 in
ASTM D149
Descriptive Properties Value Comments
Inclined Plane Tracking 107 min
UL 746/ASTM D2303
Outdoor Suitability f1
UL 746C