Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 60ANS200 Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 60ANS200 Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, translucent thermoplastic elastomer (TPE) with a relative haze of 85 to 90%. This material is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is completely recyclable.Non-hygroscopic product.Translucent.ColorableTranslucency allows trendy designs in applications such as grips, packaging.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60

@Thickness 2.00 mm
60

@Thickness 0.0787 in
ASTM D2240
Tensile Strength at Break 12.1 MPa
1750 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 1.93 MPa
280 psi
Across Flow; ASTM D412
Elongation at Break 890 %
890 %
Across Flow; ASTM D412
Tear Strength 28.0 kN/m
160 pli
73°F, Die C; ASTM D624
Processing Properties Metric English Comments
Processing Temperature 170 - 220 °C
338 - 428 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets
Users viewing this material also viewed the following: