ExxonMobil Socony Oven Conveyor Lubricant

Category Fluid , Lubricant
Manufacturer ExxonMobil
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Socony Oven Conveyor Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Socony Oven Conveyer Lubricant is a high performance product designed specifically for the lubrication of oven conveyor chains at temperatures up to 200 degrees celsius. It is formulated from a low viscosity oil and colloidal graphite. The oil acts as a carrier for the graphite and can penetrate between the moving parts.  The oil is sufficiently volatile at the working temperature to evaporate without leaving residues that might cause sticking. Socony Oven Conveyor Lubricant is best applied at a low temperature point to allow the fluid to penetrate between the links and pins.  As the conveyor moves into a hot zone the carrier evaporates, leaving a lubricating film of graphite.  The lubricant may be applied manually by brush or some form of centralised mechanical system.Socony Oven Conveyer Lubricant is an extra high performance product designed specifically for the lubrication of oven conveyor chains at temperatures up to 200ºC. Specific applications include: Fibre glass insulation manufacture; Particleboard, plastics and textiles manufacture
Physical Properties Metric English Comments
API Gravity 34.2 °
34.2 °
ASTM D4052
Kinematic Viscosity at 40°C (104°F) 13.3 cSt
13.3 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 3.7 cSt
3.7 cSt
ASTM D445
Thermal Properties Metric English Comments
Flash Point 265 °C
509 °F
ASTM D92