ExxonMobil SpectraSyn™ 10 Polyalphaolefin (PAO) Fluid

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer Exxon Chemical
Trade Name SpectraSyn™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil SpectraSyn™ 10 Polyalphaolefin (PAO) Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) products have high viscosity indices which translate to improved flow at low temperatures and increased film thickness at high temperatures. SpectraSyn™ Low Viscosity PAO products are the primary basestocks for synthetic lubricants used in passenger car engines, heavy-duty diesel engines, transmissions, gear boxes and a variety of industrial applications. Appearance: Bright & ClearAvailability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.835 g/cc

@Temperature 15.6 °C
0.0302 lb/in³

@Temperature 60.1 °F
ASTM D4052
Brookfield Viscosity 36650 cP

@Temperature -40.0 °C
36650 cP

@Temperature -40.0 °F
ASTM D2983
Viscosity Measurement 137
137
Index; ASTM D2270
Kinematic Viscosity 39000 cSt

@Temperature -40.0 °C
39000 cSt

@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 66 cSt
66 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 10 cSt
10 cSt
ASTM D445
Evaporation Loss 0.70 %

@Temperature 150 °C,
Time 79200 sec
0.70 %

@Temperature 302 °F,
Time 22.0 hour
ASTM D972
Thermal Properties Metric English Comments
Pour Point -47.8 °C
-54.0 °F
ASTM D5950/D97
Flash Point 266 °C
511 °F
COC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4615
1.4615
ASTM D1218
Electrical Properties Metric English Comments
Dielectric Breakdown 35600 V
35600 V
Chemical Properties Metric English Comments
Acid Value <= 0.050
<= 0.050
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Aniline Point 374.3°F
ASTM D611
Cold Cranking Simulator 8840 cP
-22°F, ASTM D5293
Color <0.5
ASTM D1500
Composition Water
<50 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000632 (g/cc)/°C
ASTM D1250
Fire point 565°F
COC, ASTM D92
Kauri-Butanol Value 5
ASTM D1133
Noack Volatility 0.032
ASTM D5800/DIN 51581