ExxonMobil Synesstic™ 5 Synthetic Fluid

Category Fluid , Lubricant
Manufacturer Exxon Chemical
Trade Name Synesstic™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Synesstic™ 5 Synthetic Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stability versus other Group V fluids. Synesstic™ AN products are particularly suited for use as a blendstocks in synthetic lubricant applications that require high stability under extreme operating conditions. Appearance: Bright & ClearAvailability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.908 g/cc

@Temperature 15.6 °C
0.0328 lb/in³

@Temperature 60.1 °F
ASTM D4052
Brookfield Viscosity 3950 cP

@Temperature -15.0 °C
3950 cP

@Temperature 5.00 °F
ASTM D2983
29000 cP

@Temperature -40.0 °C
29000 cP

@Temperature -40.0 °F
ASTM D2983
Viscosity Measurement 74
74
Index; ASTM D2270
Kinematic Viscosity 43600 cSt

@Temperature -40.0 °C
43600 cSt

@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 29 cSt
29 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 4.7 cSt
4.7 cSt
ASTM D445
Evaporation Loss 15.6 %

@Temperature 205 °C,
Time 23400 sec
15.6 %

@Temperature 401 °F,
Time 6.50 hour
ASTM D972
Thermal Properties Metric English Comments
Pour Point -38.9 °C
-38.0 °F
ASTM D5950/D97
Flash Point 222 °C
432 °F
COC; ASTM D92
256 °C
493 °F
PMCC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.522
1.522
ASTM D1218
Electrical Properties Metric English Comments
Dielectric Breakdown 49000 V
49000 V
Chemical Properties Metric English Comments
Acid Value <= 0.050
<= 0.050
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Aniline Point 89.6°F
ASTM D611
Bromine Number <1.3 g Br/100g
ASTM D1159 (mod)
Color <1.5
ASTM D1500
Composition Water
<50 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000527 (g/cc)/°C
ASTM D1250
Elastomer Compatibility 0
Fluoroelastomer Hardness Change, ASTM D471
0.008
Fluoroelastomer Volume Change, ASTM D471
0.019
Fluoroelastomer Tensile Strength Change, ASTM D471
-0.06
Fluoroelastomer Elongation Change, ASTM D471
-0.066
Polyacrylate Tensile Strength Change, ASTM D471
-0.09
Nitrile Hardness Change, ASTM D471
-0.11
Polyacrylate Hardness Change, ASTM D471
0.141
Nitrile Volume Change, ASTM D471
0.179
Polyacrylate Volume Change, ASTM D471
-0.256
Nitrile Elongation Change, ASTM D471
-0.272
Polyacrylate Elongation Change, ASTM D471
-0.278
Nitrile Tensile Strength Change, ASTM D471
Fire point 493°F
COC, ASTM D92
Hydrolytic Stability, TAN Change 0.02 mg KOH/g
ASTM D2619
Kauri-Butanol Value 31
ASTM D1133
Noack Volatility 0.127
ASTM D5800/DIN 51581
RPVOT >1400 min
With AO, ASTM D2272
196 min
Neat, ASTM D2272