ExxonMobil VISTANEX™ L-100

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Exxon Chemical
Trade Name VISTANEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil VISTANEX™ L-100.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
Molecular Weight 1.06e+6 - 1.34e+6 g/mol
1.06e+6 - 1.34e+6 g/mol
Viscosity average
Ash <= 0.30 %
<= 0.30 %
Collected Volatile Condensable Material <= 0.30 %
<= 0.30 %
Descriptive Properties Value Comments
Anti oxidant 0.05 ± 0.04
wt %