Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds GK 72/R Flexible PVC, Flame Retardant Sheathing Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GK 72/R Flexible PVC, Flame Retardant Sheathing Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mineral Oil resistant (75°C)
Physical Properties Metric English Comments
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1186
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 74
70 - 74
ISO R 868
Tensile Strength at Break >= 13.0 MPa
>= 1890 psi
ISO R 527
Elongation at Break >= 380 %
>= 380 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 24 %
24 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 70
CEI 20-34/3-2