Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds HL 84 Flexible PVC, Insulation for High Temperatures

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HL 84 Flexible PVC, Insulation for High Temperatures.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purposes
Physical Properties Metric English Comments
Density 1.41 - 1.45 g/cc
0.0509 - 0.0524 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 86
82 - 86
ISO R 868
Tensile Strength at Break >= 15.0 MPa
>= 2180 psi
ISO R 527
Elongation at Break >= 300 %
>= 300 %
ISO R 527
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 23.0 °C
2.00e+14 ohm-cm

@Temperature 73.4 °F
ASTM D257
Descriptive Properties Value Comments
Thermal Stability (minutes) 150
CEI 20-34/3-2
Users viewing this material also viewed the following: