Fainplast Compounds KL 0993 Flexible PVC, Insulation for High Temperatures Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds KL 0993 Flexible PVC, Insulation for High Temperatures Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Insulation
Physical Properties Metric English Comments
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92
88 - 92
ISO R 868
Tensile Strength at Break >= 16.0 MPa
>= 2320 psi
ISO R 527
Elongation at Break >= 220 %
>= 220 %
ISO R 527
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+14 ohm-cm

@Temperature 23.0 °C
5.00e+14 ohm-cm

@Temperature 73.4 °F
ASTM D257
Descriptive Properties Value Comments
Thermal Stability (minutes) 120
CEI 20-34/3-2