Fainplast Compounds PG 62/K Flexible PVC, Extrusion Modified with Rubber

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PG 62/K Flexible PVC, Extrusion Modified with Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Gaskets modified with rubber opaque surface
Physical Properties Metric English Comments
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 64
60 - 64
ISO R 868
Tensile Strength at Break 16.0 MPa
2320 psi
ISO R 527
Elongation at Break 420 %
420 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
Cold Flex; ISO 458/2