Material Notes:
Extrusion transparent films
Physical Properties Metric English Comments
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.0 MPa
5950 psi
ISO R 527
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO R527
Elongation at Break 130 %
130 %
ISO R 527
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 52.0 - 54.0 °C

@Load 5.00 kg
126 - 129 °F

@Load 11.0 lb
ISO R306
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified