Fine Organics FINALUX G 732 Lubricant Additive

Category Fluid , Lubricant , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Fine Organics
Trade Name FINALUX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fine Organics FINALUX G 732 Lubricant Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Compatible external lubricant for rigid and soft PVC with good compatibility and release properties, for use preferably in semi-rigid and soft PVC articles.Information provided by Fine Organics
Physical Properties Metric English Comments
Additive Loading 0.50 - 1.5 %
0.50 - 1.5 %
P PVC
0.50 - 1.5 %
0.50 - 1.5 %
R PVC
Descriptive Properties Value Comments
Influence on Transparency Clear
Lubricating Effect Internal/External
Physical Form Liquid