Formosa Plastics Formolene® 4101N Staple Fiber and Injection Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 4101N Staple Fiber and Injection Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101N is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general purpose injection molding applications. It contains a unique combination of stabilizers which give it process stability and end use performance.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.904 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Temperature 230 °C
12 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 38.6 MPa
5600 psi
2" (50mm) per min.; ASTM D638
Elongation at Yield 8.5 %
8.5 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Impact 0.80
0.80
ft-lb/in Notched Charpy @23°C/73°F; ASTM D256