Formosa Plastics Formolon® 10 PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® 10 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC Homopolymer Dispersion Resin F-10 is a medium molecular weight PVC homopolymer dispersion resin with low residual surfactant content. Plastisol prepared using F-10 exhibit low paste viscosity as well as excellent clarity and heat stability. Applications include sheet goods flooring wearlayer, low density chemical blow foam and strand coatingNote 1. 500 gm resin and 300 gm DOP, Hobart mixer mixed 5 min. @ No. 1 speed and 10 min. @ No. 2 speed, undeaeratedInformation provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Volatiles 0.30 %
0.30 %
ASTM D3030
Viscosity 0.98 cP
0.98 cP
Inherent; ASTM D1243
8000 cP
8000 cP
Severs, 100 psig aged 2 hrs, See note 1; SPI-VD-T2
Relative Viscosity 2.3 cP
2.3 cP
QC-10-104
Brookfield Viscosity 4500 cP
4500 cP
20 rpm aged 2 hrs, See note 1; SPI-VD-T1
6000 cP
6000 cP
2 rpm aged 2 hrs, See note 1; SPI-VD-T1
Descriptive Properties Value Comments
Composition 0.015
Methanol Extract, ASTM D2222
Gelation Temperature 158°F
SPI-VD-T18
K-Value 68
Fikentscher's Constant