Formosa Plastics Formolon® APURG Compound

Category Polymer
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® APURG Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
APURG Powder Purge Compound Series The APURG compounds are highly filled, over stabilized dry-blends designed for use in PVC extruders. The material should be used for normal cleaning purposes prior to equipment shut down. It can also be used during short periods of down time due to maintenance (or other), remaining in the equipment for these short periods, providing a clean screw area for the equipment start up.Information provided by Formosa Plastics Corporation, USA
Descriptive Properties Value Comments
Barbender heat stability >120 min
195°C and 6 rpm, ASTM D2538