Freudenberg Simrit F40 Fluorosilicone Elastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Freudenberg Simrit
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Freudenberg Simrit F40 Fluorosilicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Combines excellent low-temperature performance of silicone with improved chemical resistance. Very good resistance to military and aerospace fuels. Excellent performance in oxygen plasma environments. Avoid polar solvents, hydrocarbon fluids and phosphate ester brake fluids. Susceptible to hydrolysis by acids and bases. Limited abrasion resistance.
Mechanical Properties Metric English Comments
Hardness, Shore A 42
42
Tensile Strength, Ultimate 7.60 MPa
1100 psi
Elongation at Break 410 %
410 %
Compression Set 20 %

@Temperature 200 °C,
Time 252000 sec
20 %

@Temperature 392 °F,
Time 70.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Descriptive Properties Value Comments
Color Blue