Material Notes:
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasoline and solvents; poor resistance to alkalis and acids.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
Original Properties; ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
Original Properties; ASTM D2240
72

@Temperature 260 °C
72

@Temperature 500 °F
Air Aging, 70 hours; ASTM D2240
Tensile Strength, Ultimate 6.82 MPa
989 psi
Original Properties; ASTM D1414
6.0688 MPa

@Temperature 260 °C
880.21 psi

@Temperature 500 °F
Air Aging, 70 hours; ASTM D1414
Elongation at Break 193 %
193 %
Original Properties; ASTM D1414
140.89 %

@Temperature 260 °C
140.89 %

@Temperature 500 °F
Air Aging, 70 hours; ASTM D1414
Compression Set 41 %

@Temperature 260 °C,
Time 79200 sec
41 %

@Temperature 500 °F,
Time 22.0 hour
50 max; ASTM D395
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -48.9 °C
-56.0 °F
Retraction Temperature, TR10; ASTM D1329
Descriptive Properties Value Comments
Color Red