GEHR Plastics ECOGEHR® WPC-30PP Composite of 70% Wood Fibers and 30% Polypropylene (PP)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Wood Filled
Manufacturer GEHR Plastics Inc
Trade Name ECOGEHR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GEHR Plastics ECOGEHR® WPC-30PP Composite of 70% Wood Fibers and 30% Polypropylene (PP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wood-polymer-composites (WPC) - these materials are composites of standard polymers and wood fibers. The excellent binding of the wood fibers to the polymer gives the materials extremely high mechanical strength. The materials are weather-resistant and can optionally be given anti-bacterial, fungicidal and UV resistant properties.Information provided by GEHR Plastics, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.8 MPa
4320 psi
ASTM D1708
Elongation at Break 1.6 %
1.6 %
ASTM D1708
Modulus of Elasticity 5.18 GPa
751 ksi
ASTM D638
Izod Impact, Unnotched (ISO) 3.78 kJ/m²
1.80 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
Descriptive Properties Value Comments
Industrially Biodegradable No
Renewable Content (%) 70