GRECO ISOTHANE 2095A Poly(caprolactone)ester TPU Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer GRECO
Trade Name ISOTHANE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOTHANE 2095A Poly(caprolactone)ester TPU Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stability. These products can be injection molded, blow molded, and extruded.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength 42.0 MPa
6090 psi
ASTM D412
Tensile Strength, Yield 8.20 MPa

@Strain 50.0 %
1190 psi

@Strain 50.0 %
ASTM D412
11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
ASTM D412
25.0 MPa

@Strain 300 %
3630 psi

@Strain 300 %
ASTM D412
Elongation at Break 480 %
480 %
ASTM D412
Tear Strength 100 kN/m
571 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 10
10
ASTM D1044(Taber) H-22
Compression Set 20 %

@Temperature 23.0 °C,
Time 79200 sec
20 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
25 %

@Temperature 70.0 °C,
Time 79200 sec
25 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395