GRECO ISOTHANE 5080A Polyether TPU Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer GRECO
Trade Name ISOTHANE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOTHANE 5080A Polyether TPU Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance properties. These products can be injection molded, blow molded, and extruded. These are used for biomedical and drug administration applications.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength 37.0 MPa
5370 psi
ASTM D412
Tensile Strength, Yield 3.60 MPa

@Strain 50.0 %
522 psi

@Strain 50.0 %
ASTM D412
5.40 MPa

@Strain 100 %
783 psi

@Strain 100 %
ASTM D412
10.0 MPa

@Strain 300 %
1450 psi

@Strain 300 %
ASTM D412
Elongation at Break 620 %
620 %
ASTM D412
Tear Strength 450 kN/m
2570 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 20
20
ASTM D1044(Taber) H-22
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
30 %

@Temperature 70.0 °C,
Time 79200 sec
30 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395