Glastic GoldMemberâ„¢ Pre-tensioned Fiber Reinforcements

Category Other Engineering Material , Composite Fibers
Manufacturer Glastic
Trade Name GoldMember™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic GoldMemberâ„¢ Pre-tensioned Fiber Reinforcements.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GoldMemberâ„¢ fiber reinforcements are available in ribbon, tape and rounds that can be applied to thermoplastics and thermoset plastics, as well as wood and metals to add strength, rigidity, and flexibility without adding excessive weight.Information provided by Glastic Corporation
Physical Properties Metric English Comments
Specific Gravity 1.62 - 1.66 g/cc

@Thickness 0.508 mm
1.62 - 1.66 g/cc

@Thickness 0.0200 in
Aramid/Glass
2.191 - 2.224 g/cc

@Thickness 0.762 mm
2.191 - 2.224 g/cc

@Thickness 0.0300 in
Fiberglass Reinforced
Water Absorption 0.595 - 0.838 %

@Thickness 0.762 mm
0.595 - 0.838 %

@Thickness 0.0300 in
Fiberglass Reinforced
5.55 - 6.39 %

@Thickness 0.508 mm
5.55 - 6.39 %

@Thickness 0.0200 in
Aramid/Glass
Mechanical Properties Metric English Comments
Tensile Strength, Yield 707 - 821 MPa
102000 - 119000 psi
1"x 0.020" Aramid/Glass
1160 - 1270 MPa
169000 - 184000 psi
3/4"x 0.030" Fiberglass Reinforced
Tensile Modulus 41.9 - 49.2 GPa

@Thickness 0.762 mm
6070 - 7130 ksi

@Thickness 0.0300 in
Fiberglass Reinforced
45.6 - 50.4 GPa

@Thickness 0.508 mm
6620 - 7310 ksi

@Thickness 0.0200 in
Aramid/Glass
Descriptive Properties Value Comments
Deflection at Failure in. 1.86
Not Reinforced
2.44
0.020" Aramid/Glass, two 3/4" wide strips on bottom
2.74
0.030" Aramid, two 3/4" strips on bottom
3.5
0.030" Fiberglass, two 3/4" wide strips on bottom
Load at Failure, lbs 1260
0.020" Aramid/Glass, two 3/4" wide strips on bottom
1640
0.030" Aramid, two 3/4" wide strips on bottom
1650
0.030" Fiberglass, two 3/4" wide strips on bottom
395
Not Reinforced
Projected Deflection, 200lbs on a 60" span, in. 1.17
0.030" Aramid, two 3/4" strips on bottom
1.2
0.030" Fiberglass, two 3/4" strips on bottom
1.29
0.020" Aramid/Glass, two 3/4" strips on bottom
2.38
Not Reinforced
Users viewing this material also viewed the following: