Global 110 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global 110 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good flowInformation provided by Global Polymers
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
23/23°C; ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 18 g/10 min

@Load 6.60 kg,
Temperature 170 °C
18 g/10 min

@Load 14.6 lb,
Temperature 338 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 102 MPa
14800 psi
ASTM D638
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Forms Pellets