Global PP-3300-RC Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global PP-3300-RC Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description-medium stiffness, low melting temperatures, very good for seal Applications-thin-walled parts, audio tapes, cupsInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Ball Indentation Hardness 54.0 MPa
7830 psi
DIN 53456
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Shear Modulus 0.460 GPa
66.7 ksi
DIN 53457
Charpy Impact, Notched 0.340 J/cm²

@Temperature -23.0 °C
1.62 ft-lb/in²

@Temperature -9.40 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
Unannealed; ASTM D648