Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name VIBRON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vibron 180 Rapid is a low cement castable based on corundum with a special addition to enable a faster heating schedule. The material is supplied in two components. The B component contains the amount of water needed.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 3.15 - 3.25 g/cc
0.114 - 0.117 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
90.0 - 110 MPa

@Temperature 1500 °C
13100 - 16000 psi

@Temperature 2730 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.93 - 2.13 W/m-K

@Temperature 600 °C
13.4 - 14.8 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.95 - 2.15 W/m-K

@Temperature 100 °C
13.5 - 14.9 BTU-in/hr-ft²-°F

@Temperature 212 °F
2.12 - 2.32 W/m-K

@Temperature 1500 °C
14.7 - 16.1 BTU-in/hr-ft²-°F

@Temperature 2730 °F
Maximum Service Temperature, Air 1870 °C
3400 °F
Shrinkage -0.400 - 0.400 %

@Temperature 1500 °C
-0.400 - 0.400 %

@Temperature 2730 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 98 %
98 %
Fe2O3 <= 0.20 %
<= 0.20 %
SiO2 <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 3150 kg
Users viewing this material also viewed the following: