Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Tensile Modulus 5.00 GPa
725 ksi
ISO 527
Flexural Strength 100 MPa
14500 psi
ISO 178
Flexural Modulus 3.30 GPa
479 ksi
ISO 178
Charpy Impact Unnotched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75/A
Vicat Softening Point >= 230 °C
>= 446 °F
50N; ISO 306