Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Grupo Repol Dinalon® B1S25 G50 50% Glass Fiber Reinforced Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Grupo Repol
Trade Name Dinalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Grupo Repol Dinalon® B1S25 G50 50% Glass Fiber Reinforced Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 210 MPa
30500 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Flexural Strength 340 MPa
49300 psi
ISO 178
Flexural Modulus 13.0 GPa
1890 ksi
ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75/A
Vicat Softening Point >= 200 °C
>= 392 °F
50 N; ISO 306