H.C. Starck Grade M11 Silicon Nitride, Si3N4

Category Ceramic , Nitride
Manufacturer H.C. Starck
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Grade M11 Silicon Nitride, Si3N4.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alpha-phase > 90%, very narrow particle size distribution.Ceramic cutting toolsHeavy duty components in automotive enginesHigh performance parts for mechanical engineeringBearing components, like high precision ballsSiAlONsMetallurgy (thermocouple protection tubes, stalk tubes, crucibles)Chemical engineering, e.g. heat exchangersFunctional parts in textile machineryReleasing agent in Silicon ingot production
Physical Properties Metric English Comments
Particle Size 0.60 µm
0.60 µm
Average Particle Size/Laser Diffraction D50
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
BET