Material Notes:
A solution of polyvinyl alcohol in water, used as a base for steel quenching media. In water solution, it cools austenitized steels faster then quenching oils, hardens steels with less distortion or breakage than straight water quenches. More economical than other water-base quenchants because of the lower concentration required. Typical concentration is 5%.Information provided by Heatbath Corporation - Park Metallurgical.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 39.2 SUS
39.2 SUS
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 43.3 °C
110 °F
Upper limit of working range
Minimum Service Temperature, Air 23.9 °C
75.0 °F
Lower limit of working range