Material Notes:
Frequently used as a preheat for tool hardening or as a heating medium for continuous production hardening. Dragout is minimal because of high fluidity. Uni-Hard IR is water-soluble and non-hygroscopic. Nonferrous and precious metals as well as ferrous alloys can be treated in Uni-Hard IR.Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 549 °C
1020 °F
Maximum Service Temperature, Air 927 °C
1700 °F
Upper limit of working range
Minimum Service Temperature, Air 593 °C
1100 °F
Lower limit of working range