Henkel Alodine Magnesium Treatment Kit Touch-Up Conversion Coating

Category Fluid , Solvent
Manufacturer Henkel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Alodine Magnesium Treatment Kit Touch-Up Conversion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Alodine Magnesium Treatment Kit contains products formulated for treating magnesium alloys to produce a chromate conversion coating conforming to SAE AMS-M-3171, Type VI. The application method conforms to requirements in NAVAIR 01-1A-509 and is meant primarily for touch-up, corrosion repair processes of magnesium alloys.
Processing Properties Metric English Comments
Processing Temperature 23.0 °C
73.4 °F
Descriptive Properties Value Comments
Chemistry Chromate
Consistency Liquid
Form Ready-to-Use, Two Part
Substrate Magnesium