Henkel Alodine T 5900 Conversion Coating

Category Fluid , Solvent
Manufacturer Henkel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Alodine T 5900 Conversion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alodine T 5900 treatment is a complex trivalent chromium conversion coating formulated for treating aluminum and its alloys, metals coated with IVD aluminum, magnesium, titanium and zinc surfaces. The process provides bare ASTM-B117 salt spray resistance, and it serves as an excellent base for bonding of paint and adhesives. Neither the product itself nor the conversion coating developed by the process contains hexavalent chromium. Alodine T 5900 can be used in immersion or pressure spray washers.
Processing Properties Metric English Comments
Processing Temperature 21.0 - 32.0 °C
69.8 - 89.6 °F
Descriptive Properties Value Comments
Chemistry Tri-Chrome
Consistency Liquid
Form Concentrate
Substrate Aluminum
Magnesium
Titanium