Henkel Frekote 700-NC Mold Release Agent

Category Fluid , Lubricant
Manufacturer Henkel
Trade Name Frekote
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Frekote 700-NC Mold Release Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A non-CFC, semi permanent, multiple release polymer resin that effectively releases all thermoset resins. Versatile agent that provides slip where mold geometry problems are encountered. Cures at room temperature, gives high-gloss finish to molded parts.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 25.0 °C
0.167 hour

@Temperature 77.0 °F