Henkel Parcolac 2945 Sealer

Category Fluid , Solvent
Manufacturer Henkel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Parcolac 2945 Sealer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Parcolac 2945 is a water-emulsifiable, rust-preventive oil designed primarily for use on articles treated with a phosphate conversion coating. It can also be applied over paint-base-type iron phosphate and zinc phosphate coatings, over black oxide coatings and on bare metal.Application: Zinc Phosphate Conversion Coating
Descriptive Properties Value Comments
Chemistry Oil, Water-emulsifiable
Consistency Liquid
Form Concentrated
Substrate Ferrous