Henkel Turco Air-Tec #23 Jet Cleaner, Exterior Wash

Category Fluid , Solvent
Manufacturer Henkel
Trade Name Turco
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Turco Air-Tec #23 Jet Cleaner, Exterior Wash.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Turco Air Tec #23 is a clear, straw-colored, alkaline concentrate designed to be diluted with water to clean painted and unpainted exterior aircraft surfaces by spraying or foaming methods. Meets requirements of MIL-C-87936A, Type I.Application: Aircraft Appearance
Descriptive Properties Value Comments
Chemistry Alkaline, Water-based
Consistency Liquid
Form Concentrated
Substrate Aluminum
Ferrous
Magnesium
Non-Ferrous
Stainless Steel
Titanium