Henkel Turco Scale Gon 5 Jet Engine Cleaner

Category Fluid , Solvent
Manufacturer Henkel
Trade Name Turco
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Turco Scale Gon 5 Jet Engine Cleaner.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Turco Scale Gon 5 is an acid-activated, yellow liquid used in the Turco Jet Engine Process to condition and remove high temperature scale from jet engine parts. Approved by Rolls-Royce, GEAE and Pratt & Whitney.Application: Jet Engine Cleaning
Processing Properties Metric English Comments
Processing Temperature 80.0 - 90.0 °C

@Time 1800 sec
176 - 194 °F

@Time 0.500 hour
Descriptive Properties Value Comments
Chemistry Mildly Acidic
Consistency Liquid
Form Concentrated
Substrate Ferrous
Stainless Steel
Titanium