Material Notes:
Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When properly engineered, carbon fabric composites can achieve the strength and stiffness of metals at significant weight savings. Hexcel's carbon fabrics are compatible with various resin systems including epoxy, polyester and vinyl ester resins.Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 274 microns
10.8 mil
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 5.8
Dry
Nominal Construction (count/in) 11
Warp
11
Fill
Type of Yarn Fill Yarn: Hexcel® IM7GP 6K
Warp Yarn: Hexcel® IM7GP 6K
Weave Style Plain