Huntsman Araldite GT 7074 Bisphenol A Epoxy Solid Resin

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GT 7074 Bisphenol A Epoxy Solid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 935 to 1175. Max color is 2.Comments/Applications: Unmodified bis A "Type 4+" epoxy. Medium melt viscosity epoxy for thick film powder coatings. Outstanding adhesion; excellent impact resistance.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 97.0 - 110 °C
207 - 230 °F
Softening Range